Seo a leanas réamhrá ar shonraíochtaí agus toisí an scriú adhmaid ceann cruinn Slotted DIN 96 caighdeánach.
Raon caighdeánach: Trastomhas snáithe 1.6 mm go 8 mm, méadrach, sliotán aonair, ceann cruinn, giotán druileála adhmaid (snáithe garbh).
Príomhthoisí (mm, sonraíochtaí coitianta)
d: Trastomhas ainmniúil an tsnáithe
ds: Trastomhas slat (an chuid réidh den tslat)
dk: Trastomhas an chinn
k: Airde an chinn
n: Leithead na sliotán
t: Doimhneacht na sliotán (uasmhéid)
L: Fad ainmniúil (raon coitianta)
| d | ds (uas/nóiméad) | dk (ainm) | k | n | T (uas) | L |
| 1.6 | 1.6/1.2 | 3.2 | 1.1 | 0.4 | 0.7 | 3-12 |
| 2.0 | 2.0/1.6 | 4.0 | 1.4 | 0.5 | 0.9 | 4-16 |
| 2.5 | 2.5/2.1 | 5.0 | 1.7 | 0.6 | 1.1 | 5-20 |
| 3.0 | 3.0/2.6 | 6.0 | 2.1 | 0.8 | 1.35 | 6-25 |
| 3.5 | 3.5/3.02 | 7.0 | 2.4 | 0.8 | 1.6 | 8-30 |

Áirítear go príomha ar na hábhair choitianta le haghaidh scriú adhmaid ceann cruinn Slotted DIN 96 cruach carbóin, cruach dhosmálta agus cóimhiotal copair. Braitheann an cineál ábhair ar leith atá le roghnú ar an timpeallacht úsáide, ar riachtanais neart agus ar bhuiséad costais.
(1) Cruach Carbóin
Is é cruach carbóin an t-ábhar is coitianta a úsáidtear le haghaidh scriúnna adhmaid, a bhfuil ísealchostas, ard-neart agus feidhmíocht phróiseála maith aige. Ina measc, is é cruach ísealcharbóin an cineál is coitianta, toisc go bhfuil cion ísealcharbóin aige, tá cruas níos fearr agus feidhmíocht phróiseála níos fearr, agus go bhfuil sé oiriúnach le haghaidh foirmiú ceannteidil fuar.
(2) Cruach Dhosmálta
Cruthaíonn an dromchla scannán dlúth ocsaíd go nádúrtha, ag soláthar cosaint friotaíochta creimeadh den scoth. Níl aon chóireáil dromchla breise ag teastáil agus tá sé oiriúnach don chuid is mó de thimpeallachtaí tais agus d'iarratais lasmuigh.
(3) Cóimhiotal Práis / Copar
Cóimhiotal copair Is minic a úsáidtear scriú adhmaid ceann cruinne slotáilte DIN 96 (déanta de phrás go minic) i suíomhanna maisiúla nó feidhmiúla speisialta mar gheall ar a gcuma órga nádúrtha, friotaíocht creimeadh den scoth agus seoltacht.
| Ábhar | Tréithe | Cásanna Infheidhme |
| Prás, CuZn | Tá an chuma álainn agus órga i ndath. Tá friotaíocht maith creimeadh aige, ach tá a neart níos ísle ná cruach carbóin. | Troscán ard-deireadh, athchóiriú seandachtaí, suiteálacha ealaíne, gabhálais crua-earraí maisiúla, naisc leictreacha |
| Cré-umha | Tá a fhriotaíocht creimeadh níos fearr ná friotaíocht práis, agus tá dath donn níos dorcha ar a chuma. | Soithí, maisiúcháin lasmuigh, fosúchán dealbhóireachta |
| Mon | 2.5 | 3 | 3.5 | 4 | 4.5 | 5 | 5.5 | 6 | 7 | 8 | 10 |
| P | 1 | 12 | 1.4 | 1.6 | 1.8 | 2 | 2.2 | 2.5 | 2.8 | 3 | 3.5 |
| ds min | 2.25 | 2.75 | 3.2 | 3.7 | 4.2 | 4.7 | 5.2 | 5.7 | 6.64 | 7.64 | 9.64 |
| ds max | 2.5 | 3 | 3.5 | 4 | 4.5 | 5 | 5.5 | 6 | 7 | 8 | 10 |
| dk max | 4.63 | 5.8 | 6.75 | 7.65 | 8.6 | 9.5 | 10.5 | 11.05 | 13.35 | 15.2 | 18.9 |
| dk min | 4.23 | 5.3 | 6.25 | 7.15 | 8 | 8.9 | 9.9 | 10.35 | 12.55 | 14.4 | 18.1 |
| k uas | 1.98 | 2.37 | 2.65 | 2.95 | 3.25 | 3.5 | 3.95 | 4.34 | 4.86 | 5.5 | 6.8 |
| k nóim | 1.78 | 2.07 | 2.35 | 2.65 | 2.95 | 3.2 | 3.65 | 3.94 | 4.46 | 5.1 | 6.4 |
| n nóim | 0.6 | 0.8 | 0.9 | 1 | 12 | 12 | 1.4 | 16 | 18 | 2 | 2.5 |
| n max | 0.85 | 1.05 | 1.15 | 1.35 | 1.55 | 1.55 | 1.75 | 1.95 | 2.15 | 2.35 | 2.85 |
| r | 0.2 | 0.2 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.5 | 0.5 | 0.5 |
| t uas | 1.3 | 1.54 | 1.74 | 1.98 | 2.2 | 2.5 | 2.7 | 2.8 | 3.06 | 3.66 | 4.32 |
| t nóim | 0.9 | 1.06 | 1.26 | 1.38 | 16 | 1.9 | 2.1 | 2.2 | 2.34 | 2.94 | 3.6 |
(4) Ábhair roghnacha eile
Cóimhiotal alúmanaim
Meáchan éadrom, creimeadh-resistant, ach le neart níos ísle
Oiriúnach do thógáil sealadach, maisiú éadrom, agus socruithe taispeántais
Cóimhiotal tíotáiniam
Neart thar a bheith ard, thar a bheith creimeadh-resistant, ach le costas ard agus próiseáil deacair
Oiriúnach do réimsí speisialta ar nós aeraspáis agus trealamh leighis ard-deireadh
(1) An meirgfidh cruach carbóin Slotted scriú adhmaid ceann cruinn DIN 96 le linn iompair mhuirí?
Chun an baol a bhaineann le meirge taise-spreagtha le linn iompair a laghdú, de ghnáth glacaimid bearta cosanta cosúil le páipéar coiscthe meirge VCI + séalaithe mála plaisteacha + desiccant, ar féidir leo meirge a chosc go héifeachtach.
(2) Conas friotaíocht creimeadh scriúnna DIN 96 a mheas?
Déantar friotaíocht creimeadh a mheasúnú trí thástálacha spraeála salainn. De ghnáth is féidir le scriúnna ghalbhánuithe cruach carbóin 48-100 uair a sheasamh; is féidir le scriúnna cruach dhosmálta na céadta go dtí na mílte uair an chloig a sheasamh gan meirge.
(3) Cad ba cheart don chasmhóimint suiteála a bheith?
Braitheann an chasmhóimint ar an ábhar, an cineál adhmaid agus na coinníollacha lubrication. Mar shampla, nuair a dhéantar scriú adhmaid ceann cruinn Sliotán 4 mm cruach carbóin DIN 96 a thiomáint isteach in adhmad crua, is é an chasmhóimint mholta ná thart ar 2–3 N·m. Má sháraítear an luach seo d'fhéadfadh go sleamhnódh an sliotán nó go mbrisfidh an ceann.